These tools will no longer be maintained as of December 31, 2024. Archived website can be found here. PubMed4Hh GitHub repository can be found here. Contact NLM Customer Service if you have questions.
2. Evaluation of the mechanical properties and porcelain bond strength of cobalt-chromium dental alloy fabricated by selective laser melting. Wu L; Zhu H; Gai X; Wang Y J Prosthet Dent; 2014 Jan; 111(1):51-5. PubMed ID: 24161258 [TBL] [Abstract][Full Text] [Related]
4. Wettability and bond strength between leucite-reinforced dental porcelains and Co-Cr alloy. Yao L; Peng C; Wu J J Prosthet Dent; 2013 Dec; 110(6):515-20. PubMed ID: 24139729 [TBL] [Abstract][Full Text] [Related]
5. The effect of zinc levels in a gold-based alloy on porcelain-metal bonding. Asakura M; Kominami Y; Hayashi T; Tsuruta S; Kawai T Dent Mater; 2012 May; 28(5):e35-41. PubMed ID: 22418286 [TBL] [Abstract][Full Text] [Related]
6. Porcelain adherence vs force to failure for palladium-gallium alloys: a critique of metal-ceramic bond testing. Papazoglou E; Brantley WA Dent Mater; 1998 Mar; 14(2):112-9. PubMed ID: 10023200 [TBL] [Abstract][Full Text] [Related]
7. Effect of soldering on metal-porcelain bond strength in repaired porcelain-fused-to-metal castings. Galindo DF; Ercoli C; Graser GN; Tallents RH; Moss ME J Prosthet Dent; 2001 Jan; 85(1):88-94. PubMed ID: 11174684 [TBL] [Abstract][Full Text] [Related]
9. New approach for evaluating metal-porcelain interfacial bonding. Suansuwan N; Swain MV Int J Prosthodont; 1999; 12(6):547-52. PubMed ID: 10815609 [TBL] [Abstract][Full Text] [Related]
10. Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting. Xiang N; Xin XZ; Chen J; Wei B J Dent; 2012 Jun; 40(6):453-7. PubMed ID: 22402336 [TBL] [Abstract][Full Text] [Related]
11. Comparison of the metal-to-ceramic bond strengths of four noble alloys with press-on-metal and conventional porcelain layering techniques. Khmaj MR; Khmaj AB; Brantley WA; Johnston WM; Dasgupta T J Prosthet Dent; 2014 Nov; 112(5):1194-200. PubMed ID: 25134992 [TBL] [Abstract][Full Text] [Related]
12. Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain. Akova T; Ucar Y; Tukay A; Balkaya MC; Brantley WA Dent Mater; 2008 Oct; 24(10):1400-4. PubMed ID: 18417202 [TBL] [Abstract][Full Text] [Related]
13. Evaluation of interface characterization and adhesion of glass ceramics to commercially pure titanium and gold alloy after thermal- and mechanical-loading. Vásquez VZ; Ozcan M; Kimpara ET Dent Mater; 2009 Feb; 25(2):221-31. PubMed ID: 18718654 [TBL] [Abstract][Full Text] [Related]
14. Fusion of low-fusing porcelain to Ti-75 alloy: an experimental study. He H; Xu L; Wen N; Wang Z; Zheng X Chin J Dent Res; 2000 May; 3(1):31-3. PubMed ID: 11314338 [TBL] [Abstract][Full Text] [Related]
16. Effect of surface treatment on bond strength of Ti-10Ta-10Nb to low-fusing porcelain. Lee BA; Kim OS; Vang MS; Park YJ J Prosthet Dent; 2013 Feb; 109(2):95-105. PubMed ID: 23395335 [TBL] [Abstract][Full Text] [Related]
17. [The bonding mechanisms of base metals for metal-ceramic crown microstructure analysis of bonding agent and gold bond between porcelain and base metals]. Wang CC; Hsu CS Kaohsiung J Med Sci; 1996 Jun; 12(6):326-38. PubMed ID: 8699570 [TBL] [Abstract][Full Text] [Related]