140 related articles for article (PubMed ID: 11504433)
21. Effects of in-office tooth whiteners on hardness of tooth-colored restoratives.
Yap AU; Wattanapayungkul P
Oper Dent; 2002; 27(2):137-41. PubMed ID: 11933903
[TBL] [Abstract][Full Text] [Related]
22. Two-body and three-body wear of glass ionomer cements.
Kunzelmann KH; Bürkle V; Bauer C
Int J Paediatr Dent; 2003 Nov; 13(6):434-40. PubMed ID: 14984050
[TBL] [Abstract][Full Text] [Related]
23. Surface roughness of aesthetic restorative materials: an in vitro comparison.
Rosen M; Grossman ES; Cleaton-Jones PE; Volchansky A
SADJ; 2001 Jul; 56(7):316-20. PubMed ID: 11575115
[TBL] [Abstract][Full Text] [Related]
24. A comparison of three different methods for the quantification of the in vitro wear of dental materials.
Heintze SD; Cavalleri A; Forjanic M; Zellweger G; Rousson V
Dent Mater; 2006 Nov; 22(11):1051-62. PubMed ID: 16386293
[TBL] [Abstract][Full Text] [Related]
25. Early and long-term wear of 'fast-set' conventional glass-ionomer cements.
van Duinen RN; Kleverlaan CJ; de Gee AJ; Werner A; Feilzer AJ
Dent Mater; 2005 Aug; 21(8):716-20. PubMed ID: 16026667
[TBL] [Abstract][Full Text] [Related]
26. Influence of water exposure on three-body wear of composite restoratives.
Yap AU; Teoh SH; Tan KB
J Biomed Mater Res; 2000 Sep; 53(5):547-53. PubMed ID: 10984703
[TBL] [Abstract][Full Text] [Related]
27. Evaluation of toothbrush and generalized wear of luting materials.
Suzuki S; Minami H
Am J Dent; 2005 Oct; 18(5):311-7. PubMed ID: 16335038
[TBL] [Abstract][Full Text] [Related]
28. Curing units' ability to cure restorative composites and dual-cured composite cements under composite overlay.
Park SH; Kim SS; Cho YS; Lee CK; Noh BD
Oper Dent; 2004; 29(6):627-35. PubMed ID: 15646217
[TBL] [Abstract][Full Text] [Related]
29. Influence of shade and storage time on the flexural strength, flexural modulus, and hardness of composites used for indirect restorations.
Cesar PF; Miranda WG; Braga RR
J Prosthet Dent; 2001 Sep; 86(3):289-96. PubMed ID: 11552166
[TBL] [Abstract][Full Text] [Related]
30. Surface characteristics of aesthetic restorative materials - an SEM study.
Bagheri R; Burrow MF; Tyas MJ
J Oral Rehabil; 2007 Jan; 34(1):68-76. PubMed ID: 17207080
[TBL] [Abstract][Full Text] [Related]
31. Hardness and wear resistance of two resin composites cured with equivalent radiant exposure from a low irradiance LED and QTH light-curing units.
Ramp LC; Broome JC; Ramp MH
Am J Dent; 2006 Feb; 19(1):31-6. PubMed ID: 16555655
[TBL] [Abstract][Full Text] [Related]
32. Durability of cermet ionomer cement conditioned in different media.
el-Din IM
Egypt Dent J; 1992 Jan; 38(1):123-30. PubMed ID: 1343996
[TBL] [Abstract][Full Text] [Related]
33. Surface finish of a new hybrid aesthetic restorative material.
Yap AU; Mok BY
Oper Dent; 2002; 27(2):161-6. PubMed ID: 11933907
[TBL] [Abstract][Full Text] [Related]
34. Effect of fluoride varnishes on color stability of esthetic restorative materials.
Autio-Gold JT; Barrett AA
Oper Dent; 2004; 29(6):636-41. PubMed ID: 15646218
[TBL] [Abstract][Full Text] [Related]
35. In vitro wear evaluation of dental materials in primary teeth.
da Cunha MR; Puppin-Rontani RM; Ferracane JL; Correr-Sobrinho L
Am J Dent; 2006 Dec; 19(6):364-9. PubMed ID: 17212079
[TBL] [Abstract][Full Text] [Related]
36. Localized wear of compomer restorative materials.
Latta MA; Barkmeier WW; Wilwerding TM; Blake SM
Am J Dent; 2001 Aug; 14(4):238-40. PubMed ID: 11699744
[TBL] [Abstract][Full Text] [Related]
37. Fluoride release from aged resin composites containing fluoridated glass filler.
Itota T; Al-Naimi OT; Carrick TE; Yoshiyama M; McCabe JF
Dent Mater; 2005 Nov; 21(11):1033-8. PubMed ID: 15878618
[TBL] [Abstract][Full Text] [Related]
38. Wear of ten dental restorative materials in five wear simulators--results of a round robin test.
Heintze SD; Zappini G; Rousson V
Dent Mater; 2005 Apr; 21(4):304-17. PubMed ID: 15766577
[TBL] [Abstract][Full Text] [Related]
39. [Comparative investigation of compressive resistance of glass-cermet cements used as a core material in post-core systems].
Ersoy E; Cetiner S; Koçak F
Ankara Univ Hekim Fak Derg; 1989 Sep; 16(3):413-7. PubMed ID: 2518746
[TBL] [Abstract][Full Text] [Related]
40. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns.
Attia A; Abdelaziz KM; Freitag S; Kern M
J Prosthet Dent; 2006 Feb; 95(2):117-23. PubMed ID: 16473085
[TBL] [Abstract][Full Text] [Related]
[Previous] [Next] [New Search]