593 related articles for article (PubMed ID: 17580466)
1. Mechanical strength of an acrylic resin palatal denture base reinforced with a mesh or bundle of glass fibers.
Hedzelek W; Gajdus P
Int J Prosthodont; 2007; 20(3):311-2. PubMed ID: 17580466
[TBL] [Abstract][Full Text] [Related]
2. Effect of two methods of reinforcement on the fracture strength of interim fixed partial dentures.
Fahmy NZ; Sharawi A
J Prosthodont; 2009 Aug; 18(6):512-20. PubMed ID: 19432757
[TBL] [Abstract][Full Text] [Related]
3. Effect of glass fiber reinforcement on the flexural strength of different denture base resins.
Aydin C; Yilmaz H; Cağlar A
Quintessence Int; 2002 Jun; 33(6):457-63. PubMed ID: 12073727
[TBL] [Abstract][Full Text] [Related]
4. Comparison of mechanical strength of palatal denture bases made from various plastic materials.
Hedzelek W; Gajdus P
Int J Prosthodont; 2006; 19(2):193-4. PubMed ID: 16602370
[TBL] [Abstract][Full Text] [Related]
5. Fracture force, deflection, and toughness of acrylic denture repairs involving glass fiber reinforcement.
Kostoulas I; Kavoura VT; Frangou MJ; Polyzois GL
J Prosthodont; 2008 Jun; 17(4):257-61. PubMed ID: 18086141
[TBL] [Abstract][Full Text] [Related]
6. Evaluation of flexural resistance of a denture base acrylic resin reinforced with glass fiber and with composite resin.
da Silva LH; de Castro HL; Tango RN; de Arruda Paes Júnior TJ; Kimpara ET
Eur J Prosthodont Restor Dent; 2010 Sep; 18(3):107-10. PubMed ID: 21077418
[TBL] [Abstract][Full Text] [Related]
7. Effect of pre- and postpolymerization on flexural strength and elastic modulus of impregnated, fiber-reinforced denture base acrylic resins.
Bertassoni LE; Marshall GW; de Souza EM; Rached RN
J Prosthet Dent; 2008 Dec; 100(6):449-57. PubMed ID: 19033029
[TBL] [Abstract][Full Text] [Related]
8. Reinforcing effect of glass-fiber-reinforced composite on flexural strength at the proportional limit of denture base resin.
Tsue F; Takahashi Y; Shimizu H
Acta Odontol Scand; 2007 Jun; 65(3):141-8. PubMed ID: 17514515
[TBL] [Abstract][Full Text] [Related]
9. Flexural strength of heat-polymerized polymethyl methacrylate denture resin reinforced with glass, aramid, or nylon fibers.
John J; Gangadhar SA; Shah I
J Prosthet Dent; 2001 Oct; 86(4):424-7. PubMed ID: 11677538
[TBL] [Abstract][Full Text] [Related]
10. Flexural properties of acrylic resin polymers reinforced with unidirectional and woven glass fibers.
Vallittu PK
J Prosthet Dent; 1999 Mar; 81(3):318-26. PubMed ID: 10050121
[TBL] [Abstract][Full Text] [Related]
11. Clinical survey of acrylic resin removable denture repairs with glass-fiber reinforcement.
Narva KK; Vallittu PK; Helenius H; Yli-Urpo A
Int J Prosthodont; 2001; 14(3):219-24. PubMed ID: 11484568
[TBL] [Abstract][Full Text] [Related]
12. The effect of glass fiber reinforcement on the residual monomer content of two denture base resins.
Yilmaz H; Aydin C; Cağlar A; Yaşar A
Quintessence Int; 2003 Feb; 34(2):148-53. PubMed ID: 12666866
[TBL] [Abstract][Full Text] [Related]
13. The static strength and modulus of fiber reinforced denture base polymer.
Narva KK; Lassila LV; Vallittu PK
Dent Mater; 2005 May; 21(5):421-8. PubMed ID: 15826698
[TBL] [Abstract][Full Text] [Related]
14. Evaluation of FRC reinforcing on flexural strength of acrylic resin denture bases.
Gharehchahi J; Aghdaee NA; Kermani N
N Y State Dent J; 2010 Nov; 76(6):40-3. PubMed ID: 21226406
[TBL] [Abstract][Full Text] [Related]
15. Strength of denture base resins repaired with auto- and visible light-polymerized materials.
Faot F; da Silva WJ; da Rosa RS; Del Bel Cury AA; Garcia RC
J Prosthodont; 2009 Aug; 18(6):496-502. PubMed ID: 19432755
[TBL] [Abstract][Full Text] [Related]
16. Studies on mechanical properties of denture base material laminated with organic fiber reinforced plastics. Part I. Basic consideration of hybrid construction.
Miyairi H; Nagai M; Muramatsu A
Bull Tokyo Med Dent Univ; 1975 Dec; 22(4):273-80. PubMed ID: 776433
[TBL] [Abstract][Full Text] [Related]
17. The effect of length parameter on the repair strength of acrylic resin using fibers or metal wires.
Kostoulas IE; Kavoura VT; Frangou MJ; Polyzois GL
Gen Dent; 2008; 56(1):51-5. PubMed ID: 18254560
[TBL] [Abstract][Full Text] [Related]
18. Effect of location of glass fiber-reinforced composite reinforcement on the flexural properties of a maxillary complete denture in vitro.
Takahashi Y; Yoshida K; Shimizu H
Acta Odontol Scand; 2011 Jul; 69(4):215-21. PubMed ID: 21281056
[TBL] [Abstract][Full Text] [Related]
19. Repair of denture base resin using woven metal and glass fiber: effect of methylene chloride pretreatment.
Nagai E; Otani K; Satoh Y; Suzuki S
J Prosthet Dent; 2001 May; 85(5):496-500. PubMed ID: 11357077
[TBL] [Abstract][Full Text] [Related]
20. Flexural strengths of denture base resin repaired with autopolymerizing resin and reinforcements after thermocycle stressing.
Minami H; Suzuki S; Kurashige H; Minesaki Y; Tanaka T
J Prosthodont; 2005 Mar; 14(1):12-8. PubMed ID: 15733130
[TBL] [Abstract][Full Text] [Related]
[Next] [New Search]