162 related articles for article (PubMed ID: 21536324)
21. Evaluation of a novel multiple phase veneering ceramic.
Sinthuprasirt P; van Noort R; Moorehead R; Pollington S
Dent Mater; 2015 Apr; 31(4):443-52. PubMed ID: 25682379
[TBL] [Abstract][Full Text] [Related]
22. Comparison of two bond strength testing methodologies for bilayered all-ceramics.
Dündar M; Ozcan M; Gökçe B; Cömlekoğlu E; Leite F; Valandro LF
Dent Mater; 2007 May; 23(5):630-6. PubMed ID: 16844212
[TBL] [Abstract][Full Text] [Related]
23. Cyclic fatigue in water of veneer-framework composites for all-ceramic dental bridges.
Studart AR; Filser F; Kocher P; Lüthy H; Gauckler LJ
Dent Mater; 2007 Feb; 23(2):177-85. PubMed ID: 16492388
[TBL] [Abstract][Full Text] [Related]
24. Evaluation of a conditioning method to improve core-veneer bond strength of zirconia restorations.
Teng J; Wang H; Liao Y; Liang X
J Prosthet Dent; 2012 Jun; 107(6):380-7. PubMed ID: 22633594
[TBL] [Abstract][Full Text] [Related]
25. Analysis of subcritical crack growth in dental ceramics using fracture mechanics and fractography.
Taskonak B; Griggs JA; Mecholsky JJ; Yan JH
Dent Mater; 2008 May; 24(5):700-7. PubMed ID: 17845817
[TBL] [Abstract][Full Text] [Related]
26. Subcritical crack growth in porcelains, glass-ceramics, and glass-infiltrated alumina composite for dental restorations.
Gonzaga CC; Yoshimura HN; Cesar PF; Miranda WG
J Mater Sci Mater Med; 2009 May; 20(5):1017-24. PubMed ID: 19112607
[TBL] [Abstract][Full Text] [Related]
27. Effect of Thermomechanical and Static Loading on the Load to Fracture of Metal-Ceramic, Monolithic, and Veneered Zirconia Posterior Fixed Partial Dentures.
Lopez-Suarez C; Tobar C; Sola-Ruiz MF; Pelaez J; Suarez MJ
J Prosthodont; 2019 Feb; 28(2):171-178. PubMed ID: 30548895
[TBL] [Abstract][Full Text] [Related]
28. Fractographic analyses of zirconia-based fixed partial dentures.
Taskonak B; Yan J; Mecholsky JJ; Sertgöz A; Koçak A
Dent Mater; 2008 Aug; 24(8):1077-82. PubMed ID: 18282595
[TBL] [Abstract][Full Text] [Related]
29. Adhesion mechanisms at the interface between Y-TZP and veneering ceramic with and without modifier.
Monaco C; Tucci A; Esposito L; Scotti R
J Dent; 2014 Nov; 42(11):1473-9. PubMed ID: 25108230
[TBL] [Abstract][Full Text] [Related]
30. Slow crack growth and reliability of dental ceramics.
Gonzaga CC; Cesar PF; Miranda WG; Yoshimura HN
Dent Mater; 2011 Apr; 27(4):394-406. PubMed ID: 21185074
[TBL] [Abstract][Full Text] [Related]
31. All-ceramic fixed partial dentures. Studies on aluminum oxide- and zirconium dioxide-based ceramic systems.
Vult von Steyern P
Swed Dent J Suppl; 2005; (173):1-69. PubMed ID: 16001730
[TBL] [Abstract][Full Text] [Related]
32. Fracture Strength of Zirconia and Alumina Ceramic Crowns Supported by Implants.
Traini T; Sorrentino R; Gherlone E; Perfetti F; Bollero P; Zarone F
J Oral Implantol; 2015 Jul; 41 Spec No():352-9. PubMed ID: 24779915
[TBL] [Abstract][Full Text] [Related]
33. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics.
Borges GA; Sophr AM; de Goes MF; Sobrinho LC; Chan DC
J Prosthet Dent; 2003 May; 89(5):479-88. PubMed ID: 12806326
[TBL] [Abstract][Full Text] [Related]
34. Plastic damage induced fracture behaviors of dental ceramic layer structures subjected to monotonic load.
Wang R; Lu C; Arola D; Zhang D
J Prosthodont; 2013 Aug; 22(6):456-64. PubMed ID: 23551817
[TBL] [Abstract][Full Text] [Related]
35. Effect of Thickness, Processing Technique and Cooling Rate Protocol on the μTBS of a Bilayer Ceramic System.
de Cássia Papaiz Gonçalves F; Bottino MA; Marques de Melo RM; Assunção Souza RO
J Adhes Dent; 2015 Aug; 17(4):307-12. PubMed ID: 26258178
[TBL] [Abstract][Full Text] [Related]
36. Impact of crystallization firing process on the microstructure and flexural strength of zirconia-reinforced lithium silicate glass-ceramics.
Riquieri H; Monteiro JB; Viegas DC; Campos TMB; de Melo RM; de Siqueira Ferreira Anzaloni Saavedra G
Dent Mater; 2018 Oct; 34(10):1483-1491. PubMed ID: 29945797
[TBL] [Abstract][Full Text] [Related]
37. Load-bearing capacity and failure types of anterior zirconia crowns veneered with overpressing and layering techniques.
Stawarczyk B; Ozcan M; Roos M; Trottmann A; Sailer I; Hämmerle CH
Dent Mater; 2011 Oct; 27(10):1045-53. PubMed ID: 21820726
[TBL] [Abstract][Full Text] [Related]
38. Determination of the slow crack growth susceptibility coefficient of dental ceramics using different methods.
Gonzaga CC; Cesar PF; Miranda WG; Yoshimura HN
J Biomed Mater Res B Appl Biomater; 2011 Nov; 99(2):247-57. PubMed ID: 21714087
[TBL] [Abstract][Full Text] [Related]
39. Pressed ceramics onto zirconia. Part 2: indentation fracture and influence of cooling rate on residual stresses.
Choi JE; Waddell JN; Swain MV
Dent Mater; 2011 Nov; 27(11):1111-8. PubMed ID: 21908034
[TBL] [Abstract][Full Text] [Related]
40. Biaxial flexural strength of the bilayered disk composed of ceria-stabilized zirconia/alumina nanocomposite (Ce-TZP/A) and veneering porcelain.
Sawada T; Schille C; Wagner V; Spintzyk S; Schweizer E; Geis-Gerstorfer J
Dent Mater; 2018 Aug; 34(8):1199-1210. PubMed ID: 29793794
[TBL] [Abstract][Full Text] [Related]