441 related articles for article (PubMed ID: 23766028)
1. Performance of the experimental resins and dental nanocomposites at varying deformation rates. Kumar N; Shortall A J Investig Clin Dent; 2014 Aug; 5(3):237-42. PubMed ID: 23766028 [TBL] [Abstract][Full Text] [Related]
2. Nano-porous thermally sintered nano silica as novel fillers for dental composites. Atai M; Pahlavan A; Moin N Dent Mater; 2012 Feb; 28(2):133-45. PubMed ID: 22137937 [TBL] [Abstract][Full Text] [Related]
3. Effect of the amount of 3-methacyloxypropyltrimethoxysilane coupling agent on physical properties of dental resin nanocomposites. Sideridou ID; Karabela MM Dent Mater; 2009 Nov; 25(11):1315-24. PubMed ID: 19580996 [TBL] [Abstract][Full Text] [Related]
4. Sol-gel materials 2. Light-curing dental composites based on ormocers of cross-linking alkoxysilane methacrylates and further nano-components. Moszner N; Gianasmidis A; Klapdohr S; Fischer UK; Rheinberger V Dent Mater; 2008 Jun; 24(6):851-6. PubMed ID: 18045680 [TBL] [Abstract][Full Text] [Related]
5. Physical properties of current dental nanohybrid and nanofill light-cured resin composites. Sideridou ID; Karabela MM; Vouvoudi ECh Dent Mater; 2011 Jun; 27(6):598-607. PubMed ID: 21477852 [TBL] [Abstract][Full Text] [Related]
6. The effect of a leucite-containing ceramic filler on the abrasive wear of dental composites. Atai M; Yassini E; Amini M; Watts DC Dent Mater; 2007 Sep; 23(9):1181-7. PubMed ID: 17507087 [TBL] [Abstract][Full Text] [Related]
7. Effect of repeated preheating cycles on flexural strength of resin composites. D'Amario M; Pacioni S; Capogreco M; Gatto R; Baldi M Oper Dent; 2013; 38(1):33-8. PubMed ID: 22770484 [TBL] [Abstract][Full Text] [Related]
8. Effect of food/oral-simulating liquids on dynamic mechanical thermal properties of dental nanohybrid light-cured resin composites. Vouvoudi EC; Sideridou ID Dent Mater; 2013 Aug; 29(8):842-50. PubMed ID: 23735751 [TBL] [Abstract][Full Text] [Related]
9. The influence of nanoscale inorganic content over optical and surface properties of model composites. Salgado VE; Cavalcante LM; Silikas N; Schneider LF J Dent; 2013 Nov; 41 Suppl 5():e45-53. PubMed ID: 23748102 [TBL] [Abstract][Full Text] [Related]
10. Degree of cure and fracture properties of experimental acid-resin modified composites under wet and dry conditions. López-Suevos F; Dickens SH Dent Mater; 2008 Jun; 24(6):778-85. PubMed ID: 17980422 [TBL] [Abstract][Full Text] [Related]
11. The effect of ceramic and porous fillers on the mechanical properties of experimental dental composites. Zandinejad AA; Atai M; Pahlevan A Dent Mater; 2006 Apr; 22(4):382-7. PubMed ID: 16055180 [TBL] [Abstract][Full Text] [Related]
12. Effect of fiber diameter on flexural properties of fiber-reinforced composites. Rezvani MB; Atai M; Hamze F Indian J Dent Res; 2013; 24(2):237-41. PubMed ID: 23965454 [TBL] [Abstract][Full Text] [Related]
14. Synthesis and study of properties of dental resin composites with different nanosilica particles size. Karabela MM; Sideridou ID Dent Mater; 2011 Aug; 27(8):825-35. PubMed ID: 21592549 [TBL] [Abstract][Full Text] [Related]
15. Water sorption, solubility, and resultant change in strength among three resin-based dental composites. Kumar N; Sangi L J Investig Clin Dent; 2014 May; 5(2):144-50. PubMed ID: 23188774 [TBL] [Abstract][Full Text] [Related]
16. Conversion degree of indirect resin composites and effect of thermocycling on their physical properties. Souza RO; Ozcan M; Michida SM; de Melo RM; Pavanelli CA; Bottino MA; Soares LE; Martin AA J Prosthodont; 2010 Apr; 19(3):218-25. PubMed ID: 20040031 [TBL] [Abstract][Full Text] [Related]
17. Mechanical properties of experimental dental composites containing a combination of mesoporous and nonporous spherical silica as fillers. Samuel SP; Li S; Mukherjee I; Guo Y; Patel AC; Baran G; Wei Y Dent Mater; 2009 Mar; 25(3):296-301. PubMed ID: 18804855 [TBL] [Abstract][Full Text] [Related]
18. Mechanistic aspects of fatigue crack growth behavior in resin based dental restorative composites. Shah MB; Ferracane JL; Kruzic JJ Dent Mater; 2009 Jul; 25(7):909-16. PubMed ID: 19233460 [TBL] [Abstract][Full Text] [Related]
19. Effect of water storage, thermocycling, the incorporation and site of placement of glass-fibers on the flexural strength of veneering composite. Göhring TN; Gallo L; Lüthy H Dent Mater; 2005 Aug; 21(8):761-72. PubMed ID: 15885765 [TBL] [Abstract][Full Text] [Related]
20. Investigations on a methacrylate-based flowable composite based on the SDR™ technology. Ilie N; Hickel R Dent Mater; 2011 Apr; 27(4):348-55. PubMed ID: 21194743 [TBL] [Abstract][Full Text] [Related] [Next] [New Search]