41. Effects of cobalt-chromium alloy surface casting on resistance to deflection fatigue and surface hardness of titanium. Vallittu PK; Luotio K Int J Prosthodont; 1996; 9(6):527-32. PubMed ID: 9171490 [TBL] [Abstract][Full Text] [Related]
42. In vitro biocompatibility of CoCrMo dental alloys fabricated by selective laser melting. Hedberg YS; Qian B; Shen Z; Virtanen S; Wallinder IO Dent Mater; 2014 May; 30(5):525-34. PubMed ID: 24598762 [TBL] [Abstract][Full Text] [Related]
44. Comparative study on torsional strength, ductility and fracture characteristics of laser-welded alpha+beta Ti-6Al-7Nb alloy, CP Titanium and Co-Cr alloy dental castings. Srimaneepong V; Yoneyama T; Kobayashi E; Doi H; Hanawa T Dent Mater; 2008 Jun; 24(6):839-45. PubMed ID: 18054380 [TBL] [Abstract][Full Text] [Related]
45. Effect of heat treatment on joint properties of laser-welded Ag-Au-Cu-Pd and Co-Cr alloys. Watanabe I; Benson AP; Nguyen K J Prosthodont; 2005 Sep; 14(3):170-4. PubMed ID: 16336234 [TBL] [Abstract][Full Text] [Related]
46. Effect of deep rolling on subsurface conditions of CoCr28Mo6 wrought alloy to improve the wear resistance of endoprostheses. Herbster M; Harnisch K; Haberland E; Kriegel P; Döbberthin C; Heyn A; Döring J; Lohmann CH; Bertrand J; Halle T J Mech Behav Biomed Mater; 2021 Jun; 118():104398. PubMed ID: 33667927 [TBL] [Abstract][Full Text] [Related]
47. Microstructure, hardness, corrosion resistance and porcelain shear bond strength comparison between cast and hot pressed CoCrMo alloy for metal-ceramic dental restorations. Henriques B; Soares D; Silva FS J Mech Behav Biomed Mater; 2012 Aug; 12():83-92. PubMed ID: 22659369 [TBL] [Abstract][Full Text] [Related]
48. The wear of high-carbon metal-on-metal bearings after different heat treatments. Kinbrum A; Unsworth A Proc Inst Mech Eng H; 2008 Aug; 222(6):887-95. PubMed ID: 18935805 [TBL] [Abstract][Full Text] [Related]
49. Phase identification and incipient melting in a cast Co--Cr surgical implant alloy. Kilner T; Pilliar RM; Weatherly GC; Allibert C J Biomed Mater Res; 1982 Jan; 16(1):63-79. PubMed ID: 7056763 [TBL] [Abstract][Full Text] [Related]
50. Microstructure and wear properties of LENS deposited medical grade CoCrMo. Janaki Ram GD; Esplin CK; Stucker BE J Mater Sci Mater Med; 2008 May; 19(5):2105-11. PubMed ID: 17990083 [TBL] [Abstract][Full Text] [Related]
51. Analysis of four dental alloys following torch/centrifugal and induction/ vacuum-pressure casting procedures. Thompson GA; Luo Q; Hefti A J Prosthet Dent; 2013 Dec; 110(6):471-80. PubMed ID: 24120072 [TBL] [Abstract][Full Text] [Related]
52. Microstructure and mechanical properties of surface treated cast titanium with Nd:YAG laser. Poulon-Quintin A; Watanabe I; Watanabe E; Bertrand C Dent Mater; 2012 Sep; 28(9):945-51. PubMed ID: 22578991 [TBL] [Abstract][Full Text] [Related]
53. Wear behavior of tetragonal zirconia polycrystal versus titanium and titanium alloy. Kanbara T; Yajima Y; Yoshinari M Biomed Mater; 2011 Apr; 6(2):021001. PubMed ID: 21393812 [TBL] [Abstract][Full Text] [Related]
54. Metallurgical, surface, and corrosion analysis of Ni-Cr dental casting alloys before and after porcelain firing. Lin HY; Bowers B; Wolan JT; Cai Z; Bumgardner JD Dent Mater; 2008 Mar; 24(3):378-85. PubMed ID: 17706759 [TBL] [Abstract][Full Text] [Related]
55. Tensile strength of laser welded cobalt-chromium alloy with and without an argon atmosphere. Tartari A; Clark RK; Juszczyk AS; Radford DR Eur J Prosthodont Restor Dent; 2010 Jun; 18(2):60-5. PubMed ID: 20698419 [TBL] [Abstract][Full Text] [Related]
56. Tribological property of the cobalt-chromium femoral head with different regions of wear in total hip arthroplasty. Duong CT; Nam JS; Seo EM; Patro BP; Chang JD; Park S; Lee SS Proc Inst Mech Eng H; 2010; 224(4):541-9. PubMed ID: 20476502 [TBL] [Abstract][Full Text] [Related]
57. Effect of Ni, W and Mo on the microstructure, phases and high-temperature sliding wear performance of CoCr matrix alloys. Cui G; Liu H; Li S; Gao G; Hassani M; Kou Z Sci Technol Adv Mater; 2020; 21(1):229-241. PubMed ID: 32489482 [TBL] [Abstract][Full Text] [Related]
58. Effect of the M(s) transformation temperature on the wear behaviour of NiTi shape memory alloys for articular prosthesis. Peña J; Solano E; Mendoza A; Casals J; Planell JA; Gil FJ Biomed Mater Eng; 2005; 15(4):289-93. PubMed ID: 16010037 [TBL] [Abstract][Full Text] [Related]
59. Chemical, Physical, and Mechanical Properties and Microstructures of Laser-Sintered Co-25Cr-5Mo-5W (SP2) and W-Free Co-28Cr-6Mo Alloys for Dental Applications. Okazaki Y; Ishino A; Higuchi S Materials (Basel); 2019 Dec; 12(24):. PubMed ID: 31817292 [TBL] [Abstract][Full Text] [Related]