  • 1. Effect of surface and heat treatments on the biaxial flexural strength and phase transformation of a Y-TZP ceramic.
    Fonseca RG; Abi-Rached Fde O; da Silva FS; Henriques BA; Pinelli LA
    J Adhes Dent; 2014 Oct; 16(5):451-8. PubMed ID: 25191667
    [TBL] [Abstract][Full Text] [Related]  

  • 2. Fracture strength and microstructure of Y-TZP zirconia after different surface treatments.
    Song JY; Park SW; Lee K; Yun KD; Lim HP
    J Prosthet Dent; 2013 Oct; 110(4):274-80. PubMed ID: 24079562
    [TBL] [Abstract][Full Text] [Related]  

  • 3. Effect of particle size on the flexural strength and phase transformation of an airborne-particle abraded yttria-stabilized tetragonal zirconia polycrystal ceramic.
    Garcia Fonseca R; de Oliveira Abi-Rached F; dos Santos Nunes Reis JM; Rambaldi E; Baldissara P
    J Prosthet Dent; 2013 Dec; 110(6):510-4. PubMed ID: 24182897
    [TBL] [Abstract][Full Text] [Related]  

  • 4. Effect of surface treatments on the biaxial flexural strength, phase transformation, and surface roughness of bilayered porcelain/zirconia dental ceramics.
    Bankoğlu Güngör M; Yılmaz H; Karakoca Nemli S; Turhan Bal B; Aydın C
    J Prosthet Dent; 2015 Jun; 113(6):585-95. PubMed ID: 25858226
    [TBL] [Abstract][Full Text] [Related]  

  • 5. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics.
    Lin WS; Ercoli C; Feng C; Morton D
    J Prosthodont; 2012 Jul; 21(5):353-62. PubMed ID: 22462639
    [TBL] [Abstract][Full Text] [Related]  

  • 6. Influence of zirconia surface treatment on veneering porcelain shear bond strength after cyclic loading.
    Nishigori A; Yoshida T; Bottino MC; Platt JA
    J Prosthet Dent; 2014 Dec; 112(6):1392-8. PubMed ID: 25258263
    [TBL] [Abstract][Full Text] [Related]  

  • 7. Effect of surface treatments on the shear bond strength of luting cements to Y-TZP ceramic.
    Sciasci P; Abi-Rached FO; Adabo GL; Baldissara P; Fonseca RG
    J Prosthet Dent; 2015 Mar; 113(3):212-9. PubMed ID: 25453565
    [TBL] [Abstract][Full Text] [Related]  

  • 8. Evaluation of a conditioning method to improve core-veneer bond strength of zirconia restorations.
    Teng J; Wang H; Liao Y; Liang X
    J Prosthet Dent; 2012 Jun; 107(6):380-7. PubMed ID: 22633594
    [TBL] [Abstract][Full Text] [Related]  

  • 9. The effect of surface treatment of the interfacial surface on fatigue-related microtensile bond strength of milled zirconia to veneering porcelain.
    Harding AB; Norling BK; Teixeira EC
    J Prosthodont; 2012 Jul; 21(5):346-52. PubMed ID: 22443122
    [TBL] [Abstract][Full Text] [Related]  

  • 10. Does airborne-particle abrasion before, rather than after, zirconia sintering lead to higher mechanical strength even under aging challenge?
    Martins SB; Trindade FZ; Góes MS; Adabo GL; Dovigo LN; Fonseca RG
    J Prosthet Dent; 2020 Jan; 123(1):155-162. PubMed ID: 31027954
    [TBL] [Abstract][Full Text] [Related]  

  • 11. Mechanical properties and bonding potential of partially stabilized zirconia treated with different chemomechanical treatments.
    El-Korashy DI; El-Refai DA
    J Adhes Dent; 2014 Aug; 16(4):365-76. PubMed ID: 24892119
    [TBL] [Abstract][Full Text] [Related]  

  • 12. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles.
    Scherrer SS; Cattani-Lorente M; Vittecoq E; de Mestral F; Griggs JA; Wiskott HW
    Dent Mater; 2011 Feb; 27(2):e28-42. PubMed ID: 21056462
    [TBL] [Abstract][Full Text] [Related]  

  • 13. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading.
    Ozcan M; Melo RM; Souza RO; Machado JP; Felipe Valandro L; Botttino MA
    J Mech Behav Biomed Mater; 2013 Apr; 20():19-28. PubMed ID: 23455160
    [TBL] [Abstract][Full Text] [Related]  

  • 14. Evaluation of roughness, wettability, and morphology of an yttria-stabilized tetragonal zirconia polycrystal ceramic after different airborne-particle abrasion protocols.
    Abi-Rached FO; Martins SB; Campos JA; Fonseca RG
    J Prosthet Dent; 2014 Dec; 112(6):1385-91. PubMed ID: 25258266
    [TBL] [Abstract][Full Text] [Related]  

  • 15. Zirconia changes after grinding and regeneration firing.
    Hatanaka GR; Polli GS; Fais LMG; Reis JMDSN; Pinelli LAP
    J Prosthet Dent; 2017 Jul; 118(1):61-68. PubMed ID: 28024816
    [TBL] [Abstract][Full Text] [Related]  

  • 16. Influence of Particle and Air-Abrasion Moment on Y-TZP Surface Characterization and Bond Strength.
    Martins SB; Abi-Rached FO; Adabo GL; Baldissara P; Fonseca RG
    J Prosthodont; 2019 Jan; 28(1):e271-e278. PubMed ID: 29235196
    [TBL] [Abstract][Full Text] [Related]  

  • 17. Evaluation of self-adhesive resin cement bond strength to yttria-stabilized zirconia ceramic (Y-TZP) using four surface treatments.
    Miragaya L; Maia LC; Sabrosa CE; de Goes MF; da Silva EM
    J Adhes Dent; 2011 Oct; 13(5):473-80. PubMed ID: 21246067
    [TBL] [Abstract][Full Text] [Related]  

  • 18. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic.
    Chaiyabutr Y; McGowan S; Phillips KM; Kois JC; Giordano RA
    J Prosthet Dent; 2008 Sep; 100(3):194-202. PubMed ID: 18762031
    [TBL] [Abstract][Full Text] [Related]  

  • 19. Effect of fatigue on biaxial flexural strength of bilayered porcelain/zirconia (Y-TZP) dental ceramics.
    Yilmaz H; Nemli SK; Aydin C; Bal BT; Tıraş T
    Dent Mater; 2011 Aug; 27(8):786-95. PubMed ID: 21524790
    [TBL] [Abstract][Full Text] [Related]  

  • 20. Surface characterization of dental Y-TZP ceramic after air abrasion treatment.
    Hallmann L; Ulmer P; Reusser E; Hämmerle CH
    J Dent; 2012 Sep; 40(9):723-35. PubMed ID: 22608990
    [TBL] [Abstract][Full Text] [Related]  