These tools will no longer be maintained as of December 31, 2024. Archived website can be found here. PubMed4Hh GitHub repository can be found here. Contact NLM Customer Service if you have questions.
178 related articles for article (PubMed ID: 28772386)
1. Influence of Porous Spherical-Shaped Hydroxyapatite on Mechanical Strength and Bioactive Function of Conventional Glass Ionomer Cement. Chiu SY; Shinonaga Y; Abe Y; Harada K; Arita K Materials (Basel); 2017 Jan; 10(1):. PubMed ID: 28772386 [TBL] [Abstract][Full Text] [Related]
2. Mechanical and Functional Properties of a Novel Apatite-Ionomer Cement for Prevention and Remineralization of Dental Caries. Imataki R; Shinonaga Y; Nishimura T; Abe Y; Arita K Materials (Basel); 2019 Dec; 12(23):. PubMed ID: 31810251 [TBL] [Abstract][Full Text] [Related]
3. Effects of porous-hydroxyapatite incorporated into glass-ionomer sealants. Shinonaga Y; Arita K; Nishimura T; Chiu SY; Chiu HH; Abe Y; Sonomoto M; Harada K; Nagaoka N Dent Mater J; 2015; 34(2):196-202. PubMed ID: 25740161 [TBL] [Abstract][Full Text] [Related]
4. Glass ionomer cement with calcium-releasing particles: Effect on dentin mineral content and mechanical properties. Vilela HS; Resende MCA; Trinca RB; Scaramucci T; Sakae LO; Braga RR Dent Mater; 2024 Feb; 40(2):236-243. PubMed ID: 37981512 [TBL] [Abstract][Full Text] [Related]
5. Comparative evaluation of shear bond strength of nano-hydroxyapatite incorporated glass ionomer cement and conventional glass ionomer cement on dense synthetic hydroxyapatite disk: An in vitro study. Choudhary K; Nandlal B Indian J Dent Res; 2015; 26(2):170-5. PubMed ID: 26096112 [TBL] [Abstract][Full Text] [Related]
6. Evaluation of the effect of micro-hydroxyapatite incorporation on the diametral tensile strength of glass ionomer cements. Sharafeddin F; Karimi S; Jowkar Z J Conserv Dent; 2019; 22(3):266-269. PubMed ID: 31367111 [TBL] [Abstract][Full Text] [Related]
7. Incorporation of Hydroxyapatite into Glass Ionomer Cement (GIC) Formulated Based on Alumino-Silicate-Fluoride Glass Ceramics from Waste Materials. Wan Jusoh WN; Matori KA; Mohd Zaid MH; Zainuddin N; Ahmad Khiri MZ; Abdul Rahman NA; Abdul Jalil R; Kul E Materials (Basel); 2021 Feb; 14(4):. PubMed ID: 33670465 [TBL] [Abstract][Full Text] [Related]
8. Hydroxyapatite particle characteristics influence the enhancement of the mechanical and chemical properties of conventional restorative glass ionomer cement. Arita K; Yamamoto A; Shinonaga Y; Harada K; Abe Y; Nakagawa K; Sugiyama S Dent Mater J; 2011; 30(5):672-83. PubMed ID: 21946488 [TBL] [Abstract][Full Text] [Related]
9. Compressive Strength of Conventional Glass Ionomer Cement Modified with TiO Ivanišević A; Rajić VB; Pilipović A; Par M; Ivanković H; Baraba A Materials (Basel); 2021 Aug; 14(17):. PubMed ID: 34501056 [TBL] [Abstract][Full Text] [Related]
10. Fluoride Release From Glass Ionomer Cement Containing Fluoroapatite And Hydroxyapatite. Malik S; Ahmed MA; Choudhry Z; Mughal N; Amin M; Lone MA J Ayub Med Coll Abbottabad; 2018; 30(2):198-202. PubMed ID: 29938418 [TBL] [Abstract][Full Text] [Related]