These tools will no longer be maintained as of December 31, 2024. Archived website can be found here. PubMed4Hh GitHub repository can be found here. Contact NLM Customer Service if you have questions.


BIOMARKERS

Molecular Biopsy of Human Tumors

- a resource for Precision Medicine *

172 related articles for article (PubMed ID: 29630621)

  • 1. In vitro aging behavior of dental composites considering the influence of filler content, storage media and incubation time.
    Krüger J; Maletz R; Ottl P; Warkentin M
    PLoS One; 2018; 13(4):e0195160. PubMed ID: 29630621
    [TBL] [Abstract][Full Text] [Related]  

  • 2. Effect of food/oral-simulating liquids on dynamic mechanical thermal properties of dental nanohybrid light-cured resin composites.
    Vouvoudi EC; Sideridou ID
    Dent Mater; 2013 Aug; 29(8):842-50. PubMed ID: 23735751
    [TBL] [Abstract][Full Text] [Related]  

  • 3. Influence of artificial aging: mechanical and physicochemical properties of dental composites under static and dynamic compression.
    Gornig DC; Maletz R; Ottl P; Warkentin M
    Clin Oral Investig; 2022 Feb; 26(2):1491-1504. PubMed ID: 34453210
    [TBL] [Abstract][Full Text] [Related]  

  • 4. Filler leachability of composites stored in distilled water or artificial saliva.
    Söderholm KJ; Mukherjee R; Longmate J
    J Dent Res; 1996 Sep; 75(9):1692-9. PubMed ID: 8952623
    [TBL] [Abstract][Full Text] [Related]  

  • 5. Investigation of mechanical properties of modern dental composites after artificial aging for one year.
    Hahnel S; Henrich A; Bürgers R; Handel G; Rosentritt M
    Oper Dent; 2010; 35(4):412-9. PubMed ID: 20672725
    [TBL] [Abstract][Full Text] [Related]  

  • 6. Physico-mechanical characteristics of commercially available bulk-fill composites.
    Leprince JG; Palin WM; Vanacker J; Sabbagh J; Devaux J; Leloup G
    J Dent; 2014 Aug; 42(8):993-1000. PubMed ID: 24874951
    [TBL] [Abstract][Full Text] [Related]  

  • 7. Physical properties of current dental nanohybrid and nanofill light-cured resin composites.
    Sideridou ID; Karabela MM; Vouvoudi ECh
    Dent Mater; 2011 Jun; 27(6):598-607. PubMed ID: 21477852
    [TBL] [Abstract][Full Text] [Related]  

  • 8. The influence of nanoscale inorganic content over optical and surface properties of model composites.
    Salgado VE; Cavalcante LM; Silikas N; Schneider LF
    J Dent; 2013 Nov; 41 Suppl 5():e45-53. PubMed ID: 23748102
    [TBL] [Abstract][Full Text] [Related]  

  • 9. Dynamic mechanical thermal properties of the dental light-cured nanohybrid composite Kalore, GC: effect of various food/oral simulating liquids.
    Sideridou ID; Vouvoudi EC; Adamidou EA
    Dent Mater; 2015 Feb; 31(2):154-61. PubMed ID: 25523943
    [TBL] [Abstract][Full Text] [Related]  

  • 10. The mechanical stability of nano-hybrid composites with new methacrylate monomers for matrix compositions.
    Schmidt C; Ilie N
    Dent Mater; 2012 Feb; 28(2):152-9. PubMed ID: 22136949
    [TBL] [Abstract][Full Text] [Related]  

  • 11. Influence of artificial saliva on abrasive wear and microhardness of dental composites filled with nanoparticles.
    Mayworm CD; Camargo SS; Bastian FL
    J Dent; 2008 Sep; 36(9):703-10. PubMed ID: 18554772
    [TBL] [Abstract][Full Text] [Related]  

  • 12. Dynamic mechanical properties of dental nanofilled light-cured resin composites: Effect of food-simulating liquids.
    Vouvoudi EC; Sideridou ID
    J Mech Behav Biomed Mater; 2012 Jun; 10():87-96. PubMed ID: 22520421
    [TBL] [Abstract][Full Text] [Related]  

  • 13. Effects of age condition on the distribution and integrity of inorganic fillers in dental resin composites.
    D'Alpino PH; Svizero Nda R; Bim Júnior O; Valduga CJ; Graeff CF; Sauro S
    Clin Oral Investig; 2016 Jun; 20(5):1011-9. PubMed ID: 26388405
    [TBL] [Abstract][Full Text] [Related]  

  • 14. The effect of a leucite-containing ceramic filler on the abrasive wear of dental composites.
    Atai M; Yassini E; Amini M; Watts DC
    Dent Mater; 2007 Sep; 23(9):1181-7. PubMed ID: 17507087
    [TBL] [Abstract][Full Text] [Related]  

  • 15. Effect of continuous longitudinal glass fiber reinforcement on the cantilever beam strength of particulate filler composites.
    Kim SH; Christopher Watts D
    Acta Odontol Scand; 2006 Nov; 64(6):383-90. PubMed ID: 17123916
    [TBL] [Abstract][Full Text] [Related]  

  • 16. Resin composite characterizations following a simplified protocol of accelerated aging as a function of the expiration date.
    D'Alpino PH; Vismara MV; Mello LM; Di Hipólito V; González AH; Graeff CF
    J Mech Behav Biomed Mater; 2014 Jul; 35():59-69. PubMed ID: 24747096
    [TBL] [Abstract][Full Text] [Related]  

  • 17. Post-irradiation hardness development, chemical softening, and thermal stability of bulk-fill and conventional resin-composites.
    Alshali RZ; Salim NA; Satterthwaite JD; Silikas N
    J Dent; 2015 Feb; 43(2):209-18. PubMed ID: 25511301
    [TBL] [Abstract][Full Text] [Related]  

  • 18. Influence of filler charge on gloss of composite materials before and after in vitro toothbrushing.
    Jassé FF; de Campos EA; Lefever D; Di Bella E; Salomon JP; Krejci I; Ardu S
    J Dent; 2013 Nov; 41 Suppl 5():e41-4. PubMed ID: 23649047
    [TBL] [Abstract][Full Text] [Related]  

  • 19. Long-term sorption and solubility of bulk-fill and conventional resin-composites in water and artificial saliva.
    Alshali RZ; Salim NA; Satterthwaite JD; Silikas N
    J Dent; 2015 Dec; 43(12):1511-8. PubMed ID: 26455541
    [TBL] [Abstract][Full Text] [Related]  

  • 20. Factors involved in mechanical fatigue degradation of dental resin composites.
    Lohbauer U; Belli R; Ferracane JL
    J Dent Res; 2013 Jul; 92(7):584-91. PubMed ID: 23694927
    [TBL] [Abstract][Full Text] [Related]  

    [Next]    [New Search]
    of 9.