8. Fracture Load of Different Zirconia Types: A Mastication Simulation Study. Abdulmajeed A; Sulaiman T; Abdulmajeed A; Bencharit S; Närhi T J Prosthodont; 2020 Dec; 29(9):787-791. PubMed ID: 32840940 [TBL] [Abstract][Full Text] [Related]
9. Effect of masticatory simulation on the translucency of different types of dental zirconia. Alraheam IA; Donovan TE; Rodgers B; Boushell L; Sulaiman TA J Prosthet Dent; 2019 Oct; 122(4):404-409. PubMed ID: 30928224 [TBL] [Abstract][Full Text] [Related]
10. Fracture load of two thicknesses of different zirconia types after fatiguing and thermocycling. Alraheam IA; Donovan T; Boushell L; Cook R; Ritter AV; Sulaiman TA J Prosthet Dent; 2020 Apr; 123(4):635-640. PubMed ID: 31383533 [TBL] [Abstract][Full Text] [Related]
11. Mechanical behavior and microstructural characterization of different zirconia polycrystals in different thicknesses. Arcila LVC; Ramos NC; Campos TMB; Dapieve KS; Valandro LF; de Melo RM; Bottino MA J Adv Prosthodont; 2021 Dec; 13(6):385-395. PubMed ID: 35003554 [TBL] [Abstract][Full Text] [Related]
12. Impact of hydrothermal aging on the light transmittance and flexural strength of colored yttria-stabilized zirconia materials of different formulations. Lümkemann N; Stawarczyk B J Prosthet Dent; 2021 Mar; 125(3):518-526. PubMed ID: 32199639 [TBL] [Abstract][Full Text] [Related]
13. Translucent zirconia in the ceramic scenario for monolithic restorations: A flexural strength and translucency comparison test. Carrabba M; Keeling AJ; Aziz A; Vichi A; Fabian Fonzar R; Wood D; Ferrari M J Dent; 2017 May; 60():70-76. PubMed ID: 28274651 [TBL] [Abstract][Full Text] [Related]
14. Lithium disilicate glass-ceramic vs translucent zirconia polycrystals bonded to distinct substrates: Fatigue failure load, number of cycles for failure, survival rates, and stress distribution. Pereira GKR; Graunke P; Maroli A; Zucuni CP; Prochnow C; Valandro LF; Caldas RA; Bacchi A J Mech Behav Biomed Mater; 2019 Mar; 91():122-130. PubMed ID: 30579109 [TBL] [Abstract][Full Text] [Related]
15. Advanced lithium disilicate: A comparative evaluation of translucency and fatigue failure load to other ceramics for monolithic restorations. Freitas JS; Souza LFB; Dellazzana FZ; Silva TMRD; Ribeiro L; Pereira GKR; May LG J Mech Behav Biomed Mater; 2023 Dec; 148():106192. PubMed ID: 37865017 [TBL] [Abstract][Full Text] [Related]
16. Strength and phase transformation of different zirconia types after chairside adjustment. Abdulmajeed A; Sulaiman TA; Abdulmajeed AA; Närhi TO J Prosthet Dent; 2024 Aug; 132(2):455-463. PubMed ID: 35934577 [TBL] [Abstract][Full Text] [Related]
17. Graded Ultra-Translucent Zirconia (5Y-PSZ) for Strength and Functionalities. Mao L; Kaizer MR; Zhao M; Guo B; Song YF; Zhang Y J Dent Res; 2018 Oct; 97(11):1222-1228. PubMed ID: 29694258 [TBL] [Abstract][Full Text] [Related]
18. Bond strength of lithium disilicate to polyetheretherketone. Sloan R; Hollis W; Selecman A; Jain V; Versluis A J Prosthet Dent; 2022 Dec; 128(6):1351-1357. PubMed ID: 33846011 [TBL] [Abstract][Full Text] [Related]
19. Impact of varying step-stress protocols on the fatigue behavior of 3Y-TZP, 4Y-TZP and 5Y-TZP ceramic. Jerman E; Lümkemann N; Eichberger M; Hampe R; Stawarczyk B Dent Mater; 2021 Jul; 37(7):1073-1082. PubMed ID: 33849757 [TBL] [Abstract][Full Text] [Related]
20. Effects of cementation surface modifications on fracture resistance of zirconia. Srikanth R; Kosmac T; Della Bona A; Yin L; Zhang Y Dent Mater; 2015 Apr; 31(4):435-42. PubMed ID: 25687628 [TBL] [Abstract][Full Text] [Related] [Next] [New Search]