250 related articles for article (PubMed ID: 34448074)
1. Effect of finishing/polishing techniques and aging on topography, C. albicans adherence, and flexural strength of ultra-translucent zirconia: an in situ study.
de Carvalho IHG; da Silva NR; Vila-Nova TEL; de Fatima Dantas de Almeida L; Veríssimo AH; de Melo RM; Zhang Y; de Assunção E Souza RO
Clin Oral Investig; 2022 Jan; 26(1):889-900. PubMed ID: 34448074
[TBL] [Abstract][Full Text] [Related]
2. Effect of finishing/polishing techniques and low temperature degradation on the surface topography, phase transformation and flexural strength of ultra-translucent ZrO
Vila-Nova TEL; Gurgel de Carvalho IH; Moura DMD; Batista AUD; Zhang Y; Paskocimas CA; Bottino MA; de Assunção E Souza RO
Dent Mater; 2020 Apr; 36(4):e126-e139. PubMed ID: 32008750
[TBL] [Abstract][Full Text] [Related]
3. Effect of Two Polishing Systems on Surface Roughness, Topography, and Flexural Strength of a Monolithic Lithium Disilicate Ceramic.
Mohammadibassir M; Rezvani MB; Golzari H; Moravej Salehi E; Fahimi MA; Kharazi Fard MJ
J Prosthodont; 2019 Jan; 28(1):e172-e180. PubMed ID: 28273681
[TBL] [Abstract][Full Text] [Related]
4. Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia.
Mohammadi-Bassir M; Babasafari M; Rezvani MB; Jamshidian M
J Prosthet Dent; 2017 Nov; 118(5):658-665. PubMed ID: 28385438
[TBL] [Abstract][Full Text] [Related]
5. The effect of surface treatments on dental zirconia: An analysis of biaxial flexural strength, surface roughness and phase transformation.
Botelho MG; Dangay S; Shih K; Lam WYH
J Dent; 2018 Aug; 75():65-73. PubMed ID: 29842902
[TBL] [Abstract][Full Text] [Related]
6. Comparative effects of glazing versus polishing on mechanical, optical, and surface properties of zirconia ceramics with different translucencies.
Jamali M; Ezoji F; Esmaeili B; Khafri S
Clin Exp Dent Res; 2024 Jun; 10(3):e884. PubMed ID: 38798053
[TBL] [Abstract][Full Text] [Related]
7. The effects of surface grinding and polishing on the phase transformation and flexural strength of zirconia.
Lee JY; Jang GW; Park II; Heo YR; Son MK
J Adv Prosthodont; 2019 Feb; 11(1):1-6. PubMed ID: 30847043
[TBL] [Abstract][Full Text] [Related]
8. Comparative effects of tungsten, diamond burs and laser for residual adhesive removal after orthodontic debonding on flexural strength, surface roughness and phase transformation of high-translucent zirconia: An in vitro study.
Babaee Hemmati Y; Neshandar Asil H; Falahchai M; Safari N
Int Orthod; 2022 Sep; 20(3):100665. PubMed ID: 35851494
[TBL] [Abstract][Full Text] [Related]
9. Strength of a Zirconia- Reinforced Glass-Ceramic After Diamond Bur Adjustment.
Moura Pereira B; Restani Oliveira A; Leal do Prado R; Gomes de Carvalho AB; Marques de Melo R; Singh Jodha K; Salazar Marocho SM; Ávila Galhano G
Eur J Prosthodont Restor Dent; 2023 Nov; 31(4):398-406. PubMed ID: 37382338
[TBL] [Abstract][Full Text] [Related]
10. The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging.
Hatanaka GR; Polli GS; Adabo GL
J Prosthet Dent; 2020 Feb; 123(2):330-337. PubMed ID: 31079884
[TBL] [Abstract][Full Text] [Related]
11. Effects of different surface finishing protocols for zirconia on surface roughness and bacterial biofilm formation.
Lee DH; Mai HN; Thant PP; Hong SH; Kim J; Jeong SM; Lee KW
J Adv Prosthodont; 2019 Feb; 11(1):41-47. PubMed ID: 30847048
[TBL] [Abstract][Full Text] [Related]
12. Surface Roughness of Monolithic and Layered Zirconia Restorations at Different Stages of Finishing and Polishing: An In Vitro Study.
Al Hamad KQ; Abu Al-Addous AM; Al-Wahadni AM; Baba NZ; Goodacre BJ
J Prosthodont; 2019 Aug; 28(7):818-825. PubMed ID: 31066483
[TBL] [Abstract][Full Text] [Related]
13. Surface Topography, Gloss and Flexural Strength of Pressable Ceramic After Finishing-Polishing Protocols.
Silva FP; Vilela ALR; Almeida MMG; Oliveira ARF; Raposo LHA; Menezes MS
Braz Dent J; 2019; 30(2):164-170. PubMed ID: 30970060
[TBL] [Abstract][Full Text] [Related]
14. Effect of air-abrasion regimens and fine diamond bur grinding on flexural strength, Weibull modulus and phase transformation of zirconium dioxide.
Michida SM; Kimpara ET; dos Santos C; Souza RO; Bottino MA; Özcan M
J Appl Biomater Funct Mater; 2015 Oct; 13(3):e266-73. PubMed ID: 26391866
[TBL] [Abstract][Full Text] [Related]
15. Simulated clinical adjustment and intra-oral polishing of two translucent, monolithic zirconia dental ceramics: An in vitro investigation of surface roughness.
Jum'ah AA; Brunton PA; Li KC; Waddell JN
J Dent; 2020 Oct; 101():103447. PubMed ID: 32763368
[TBL] [Abstract][Full Text] [Related]
16. The adverse effects of tungsten carbide grinding on the strength of dental zirconia.
Wang Y; Lam WYH; Luk HWK; Øilo M; Shih K; Botelho MG
Dent Mater; 2020 Apr; 36(4):560-569. PubMed ID: 32063392
[TBL] [Abstract][Full Text] [Related]
17. The effect of adjustment and finishing procedure on roughness, strength, and phase transformation of monolithic zirconia.
Ozturk I; Caglar I; Duymus ZY
Clin Oral Investig; 2022 Jul; 26(7):4761-4768. PubMed ID: 35292846
[TBL] [Abstract][Full Text] [Related]
18. Effect of Surface Modification on In-Depth Transformations and Flexural Strength of Zirconia Ceramics.
Wongkamhaeng K; Dawson DV; Holloway JA; Denry I
J Prosthodont; 2019 Jan; 28(1):e364-e375. PubMed ID: 29741238
[TBL] [Abstract][Full Text] [Related]
19. Microstructural analysis and reliability of monolithic zirconia after simulated adjustment protocols.
Chun EP; Anami LC; Bonfante EA; Bottino MA
Dent Mater; 2017 Aug; 33(8):934-943. PubMed ID: 28606409
[TBL] [Abstract][Full Text] [Related]
20. A Comparative Study on Simulated Chairside Grinding and Polishing of Monolithic Zirconia.
Kheur M; Lakha T; Shaikh S; Kheur S; Qamri B; Zhen LW; Al-Haj Husain N; Özcan M
Materials (Basel); 2022 Mar; 15(6):. PubMed ID: 35329653
[TBL] [Abstract][Full Text] [Related]