156 related articles for article (PubMed ID: 36837336)
1. Gradient Microstructure and Texture Formation in a Metastable Austenitic Stainless Steel during Cold Rotary Swaging.
Panov D; Kudryavtsev E; Naumov S; Klimenko D; Chernichenko R; Mirontsov V; Stepanov N; Zherebtsov S; Salishchev G; Pertcev A
Materials (Basel); 2023 Feb; 16(4):. PubMed ID: 36837336
[TBL] [Abstract][Full Text] [Related]
2. Effect of Cold Swaging on the Bulk Gradient Structure Formation and Mechanical Properties of a 316-Type Austenitic Stainless Steel.
Panov D; Chernichenko R; Kudryavtsev E; Klimenko D; Naumov S; Pertcev A
Materials (Basel); 2022 Mar; 15(7):. PubMed ID: 35407801
[TBL] [Abstract][Full Text] [Related]
3. Affecting Microstructure and Properties of Additively Manufactured AISI 316L Steel by Rotary Swaging.
Kunčická L; Kocich R; Benč M; Dvořák J
Materials (Basel); 2022 Sep; 15(18):. PubMed ID: 36143603
[TBL] [Abstract][Full Text] [Related]
4. Investigation of microstructure evolution and martensite transformation developed in austenitic stainless steel subjected to a plastic strain gradient: A combination study of Mirco-XRD, EBSD, and ECCI techniques.
Berahmand M; Ketabchi M; Jamshidian M; Tsurekawa S
Micron; 2021 Apr; 143():103014. PubMed ID: 33549854
[TBL] [Abstract][Full Text] [Related]
5. Effect of Rolling Temperature on Microstructure Evolution and Mechanical Properties of AISI316LN Austenitic Stainless Steel.
Xiong Y; Yue Y; He T; Lu Y; Ren F; Cao W
Materials (Basel); 2018 Aug; 11(9):. PubMed ID: 30158476
[TBL] [Abstract][Full Text] [Related]
6. Warm Pre-Strain: Strengthening the Metastable 304L Austenitic Stainless Steel without Compromising Its Hydrogen Embrittlement Resistance.
Wang Y; Zhou Z; Wu W; Gong J
Materials (Basel); 2017 Nov; 10(11):. PubMed ID: 29160830
[TBL] [Abstract][Full Text] [Related]
7. Metastable Austenitic Steel Structure and Mechanical Properties Evolution in the Process of Cold Radial Forging.
Panov D; Pertsev A; Smirnov A; Khotinov V; Simonov Y
Materials (Basel); 2019 Jun; 12(13):. PubMed ID: 31248031
[TBL] [Abstract][Full Text] [Related]
8. Texture and Differential Stress Development in W/Ni-Co Composite after Rotary Swaging.
Strunz P; Kocich R; Canelo-Yubero D; Macháčková A; Beran P; Krátká L
Materials (Basel); 2020 Jun; 13(12):. PubMed ID: 32604904
[TBL] [Abstract][Full Text] [Related]
9. Phase Transformation in 316L Austenitic Steel Induced by Fracture at Cryogenic Temperatures: Experiment and Modelling.
Nalepka K; Skoczeń B; Ciepielowska M; Schmidt R; Tabin J; Schmidt E; Zwolińska-Faryj W; Chulist R
Materials (Basel); 2020 Dec; 14(1):. PubMed ID: 33396788
[TBL] [Abstract][Full Text] [Related]
10. Effects of strain and strain-induced α'-martensite on passive films in AISI 304 austenitic stainless steel.
Lv J; Luo H
Mater Sci Eng C Mater Biol Appl; 2014 Jan; 34():484-90. PubMed ID: 24268285
[TBL] [Abstract][Full Text] [Related]
11. High Cycle Fatigue Behaviour of 316L Stainless Steel Produced via Selective Laser Melting Method and Post Processed by Hot Rotary Swaging.
Opěla P; Benč M; Kolomy S; Jakůbek Z; Beranová D
Materials (Basel); 2023 Apr; 16(9):. PubMed ID: 37176281
[TBL] [Abstract][Full Text] [Related]
12. Comparison of conventional and severe shot peening effects on the microstructure, texture, roughness, hardness, and electrochemical behavior of austenitic stainless steel.
Yazdani F; Rabiee SM; Jamaati R
Heliyon; 2024 May; 10(10):e31284. PubMed ID: 38803990
[TBL] [Abstract][Full Text] [Related]
13. Rate effects on transformation kinetics in a metastable austenitic stainless steel.
Alturk R; Luecke WE; Mates S; Araujo A; Raghavan KS; Abu-Farha F
Procedia Eng; 2017; 207():. PubMed ID: 33029261
[TBL] [Abstract][Full Text] [Related]
14. Advantageous Implications of Reversed Austenite for the Tensile Properties of Super 13Cr Martensitic Stainless Steel.
Wang P; Zheng W; Yu X; Wang Y
Materials (Basel); 2022 Nov; 15(21):. PubMed ID: 36363289
[TBL] [Abstract][Full Text] [Related]
15. Dissimilar Laser Welding of Austenitic Stainless Steel and Abrasion-Resistant Steel: Microstructural Evolution and Mechanical Properties Enhanced by Post-Weld Heat Treatment.
Hietala M; Jaskari M; Ali M; Järvenpää A; Hamada A
Materials (Basel); 2021 Sep; 14(19):. PubMed ID: 34639977
[TBL] [Abstract][Full Text] [Related]
16. Effect of Shear Strain Rate on Microstructure and Properties of Austenitic Steel Processed by Cyclic Forward/Reverse Torsion.
Zhang Z; Dong Q; Song B; He H; Chai L; Guo N; Wang B; Yao Z
Materials (Basel); 2019 Feb; 12(3):. PubMed ID: 30736410
[TBL] [Abstract][Full Text] [Related]
17. Microstructure Evolution at Ni/Fe Interface in Dissimilar Metal Weld between Ferritic Steel and Austenitic Stainless Steel.
Li X; Nie J; Wang X; Li K; Zhang H
Materials (Basel); 2023 Sep; 16(18):. PubMed ID: 37763571
[TBL] [Abstract][Full Text] [Related]
18. Manufacturing of high-strength Ni-free Co-Cr-Mo alloy rods via cold swaging.
Yamanaka K; Mori M; Yoshida K; Kuramoto K; Chiba A
J Mech Behav Biomed Mater; 2016 Jul; 60():38-47. PubMed ID: 26773647
[TBL] [Abstract][Full Text] [Related]
19. Hydrogen-Induced Delayed Cracking in TRIP-Aided Lean-Alloyed Ferritic-Austenitic Stainless Steels.
Papula S; Sarikka T; Anttila S; Talonen J; Virkkunen I; Hänninen H
Materials (Basel); 2017 Jun; 10(6):. PubMed ID: 28772975
[TBL] [Abstract][Full Text] [Related]
20. Compressive Behavior and Constitutive Model of Austenitic Stainless Steel S30403 in High Strain Range.
Peng Y; Chu J; Dong J
Materials (Basel); 2018 Jun; 11(6):. PubMed ID: 29914083
[TBL] [Abstract][Full Text] [Related]
[Next] [New Search]