1. Comparison of tensile properties and porcelain bond strength in metal frameworks fabricated by selective laser melting using three different Co-Cr alloy powders. Yildiz MT; Babacan N J Prosthet Dent; 2024 May; 131(5):936-942. PubMed ID: 38042642 [TBL] [Abstract][Full Text] [Related]
2. Evaluation of the mechanical properties and porcelain bond strength of cobalt-chromium dental alloy fabricated by selective laser melting. Wu L; Zhu H; Gai X; Wang Y J Prosthet Dent; 2014 Jan; 111(1):51-5. PubMed ID: 24161258 [TBL] [Abstract][Full Text] [Related]
3. Effects of heat treatment on metal-ceramic combination of selective-laser-melted cobalt-chromium alloy. Yan X; Xu YX; Wu Y; Lin H J Prosthet Dent; 2018 Aug; 120(2):319.e1-319.e6. PubMed ID: 30097265 [TBL] [Abstract][Full Text] [Related]
4. Bond strengths of porcelain to cobalt-chromium alloys made by casting, milling, and selective laser melting. Li J; Chen C; Liao J; Liu L; Ye X; Lin S; Ye J J Prosthet Dent; 2017 Jul; 118(1):69-75. PubMed ID: 27927283 [TBL] [Abstract][Full Text] [Related]
5. Effects of post-treatment on metal-ceramic bond properties of selective laser melted Co-Cr dental alloy. Part 1: Annealing temperature. Zhou Y; Dong X; Li N; Yan J J Prosthet Dent; 2023 Apr; 129(4):657.e1-657.e9. PubMed ID: 36842952 [TBL] [Abstract][Full Text] [Related]
6. Evaluation of the relationship between metallurgical properties and metal-ceramic bond characteristics of Co-Cr alloys manufactured by different techniques. Altuntas MC; Guleryuz A J Prosthet Dent; 2023 Dec; 130(6):937.e1-937.e10. PubMed ID: 37806942 [TBL] [Abstract][Full Text] [Related]
7. Chemical composition, surface roughness, and ceramic bond strength of additively manufactured cobalt-chromium dental alloys. Revilla-León M; Al-Haj Husain N; Methani MM; Özcan M J Prosthet Dent; 2021 May; 125(5):825-831. PubMed ID: 32466963 [TBL] [Abstract][Full Text] [Related]
8. Evaluation of metal-ceramic bond characteristics of three dental Co-Cr alloys prepared with different fabrication techniques. Wang H; Feng Q; Li N; Xu S J Prosthet Dent; 2016 Dec; 116(6):916-923. PubMed ID: 27460313 [TBL] [Abstract][Full Text] [Related]
9. Microstructural and mechanical characterization of six Co-Cr alloys made by conventional casting and selective laser melting. Al Jabbari YS; Dimitriadis K; Sufyan A; Zinelis S J Prosthet Dent; 2024 Sep; 132(3):646.e1-646.e10. PubMed ID: 38955601 [TBL] [Abstract][Full Text] [Related]
10. Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain. Akova T; Ucar Y; Tukay A; Balkaya MC; Brantley WA Dent Mater; 2008 Oct; 24(10):1400-4. PubMed ID: 18417202 [TBL] [Abstract][Full Text] [Related]
11. Comparative analysis of the microstructures and mechanical properties of Co-Cr dental alloys fabricated by different methods. Zhou Y; Li N; Yan J; Zeng Q J Prosthet Dent; 2018 Oct; 120(4):617-623. PubMed ID: 29627206 [TBL] [Abstract][Full Text] [Related]
12. Recycling selective laser melting alloy powder on cobalt chromium-to-ceramic bond strength. Albayrak H; Ayata M; Demirel B J Prosthet Dent; 2023 Nov; 130(5):786.e1-786.e7. PubMed ID: 37718178 [TBL] [Abstract][Full Text] [Related]
13. Effect of layered manufacturing techniques, alloy powders, and layer thickness on metal-ceramic bond strength. Ekren O; Ozkomur A; Ucar Y J Prosthet Dent; 2018 Mar; 119(3):481-487. PubMed ID: 28689902 [TBL] [Abstract][Full Text] [Related]
14. Analysis of microstructure and fatigue of cast versus selective laser-melted dental Co-Cr alloy. Wu M; Dong X; Qu Y; Yan J; Li N J Prosthet Dent; 2022 Aug; 128(2):218.e1-218.e7. PubMed ID: 35786348 [TBL] [Abstract][Full Text] [Related]
15. Comparison of the metal-ceramic bond after recasting and after laser sintering. Kul E; Aladag LI; Duymus ZY J Prosthet Dent; 2015 Jul; 114(1):109-13. PubMed ID: 25858225 [TBL] [Abstract][Full Text] [Related]
16. Evaluation of mechanical properties and porcelain bonded strength of nickel-chromium dental alloy fabricated by laser rapid forming. Liu Y; Wang Z; Gao B; Zhao X; Lin X; Wu J Lasers Med Sci; 2010 Nov; 25(6):799-804. PubMed ID: 19548056 [TBL] [Abstract][Full Text] [Related]
17. Effects of multiple firings on metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting. Ren XW; Zeng L; Wei ZM; Xin XZ; Wei B J Prosthet Dent; 2016 Jan; 115(1):109-14. PubMed ID: 26372627 [TBL] [Abstract][Full Text] [Related]
18. Effect of laser etching on surface characteristics and porcelain bond to soft milled and direct metal laser sintered cobalt chromium alloys. AboElhassan RG; Morsy N J Prosthet Dent; 2024 Jul; 132(1):269.e1-269.e6. PubMed ID: 38609765 [TBL] [Abstract][Full Text] [Related]
19. Effect of PFM Firing Cycles on the Mechanical Properties, Phase Composition, and Microstructure of Nickel-Chromium Alloy. Anwar M; Tripathi A; Kar SK; Sekhar KC J Prosthodont; 2015 Dec; 24(8):634-41. PubMed ID: 26215348 [TBL] [Abstract][Full Text] [Related]
20. Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting. Xiang N; Xin XZ; Chen J; Wei B J Dent; 2012 Jun; 40(6):453-7. PubMed ID: 22402336 [TBL] [Abstract][Full Text] [Related] [Next] [New Search]