  • 1. The effect of pH on the in vitro degradation of poly(glycolide lactide) copolymer absorbable sutures.
    Chu CC
    J Biomed Mater Res; 1982 Mar; 16(2):117-24. PubMed ID: 7061530
    [TBL] [Abstract][Full Text] [Related]  

  • 2. A comparison of the effect of pH on the biodegradation of two synthetic absorbable sutures.
    Chu CC
    Ann Surg; 1982 Jan; 195(1):55-9. PubMed ID: 6275809
    [TBL] [Abstract][Full Text] [Related]  

  • 3. The in-vitro degradation of poly(glycolic acid) sutures--effect of pH.
    Chu CC
    J Biomed Mater Res; 1981 Nov; 15(6):795-804. PubMed ID: 6273445
    [TBL] [Abstract][Full Text] [Related]  

  • 4. Plasma surface modification of synthetic absorbable sutures.
    Loh IH; Lin HL; Chu CC
    J Appl Biomater; 1992; 3(2):131-46. PubMed ID: 10147710
    [TBL] [Abstract][Full Text] [Related]  

  • 5. In-vivo comparison of four absorbable sutures: Vicryl, Dexon Plus, Maxon and PDS.
    Bourne RB; Bitar H; Andreae PR; Martin LM; Finlay JB; Marquis F
    Can J Surg; 1988 Jan; 31(1):43-5. PubMed ID: 2827875
    [TBL] [Abstract][Full Text] [Related]  

  • 6. Effect of a combined gamma irradiation and Parylene plasma treatment on the hydrolytic degradation of synthetic biodegradable sutures.
    Zhang L; Chu CC; Loh IH
    J Biomed Mater Res; 1993 Nov; 27(11):1425-41. PubMed ID: 8263005
    [TBL] [Abstract][Full Text] [Related]  

  • 7. An in-vitro study of the effect of buffer on the degradation of poly(glycolic acid) sutures.
    Chu CC
    J Biomed Mater Res; 1981 Jan; 15(1):19-27. PubMed ID: 6294120
    [TBL] [Abstract][Full Text] [Related]  

  • 8. The pH dependence of monofilament sutures on hydrolytic degradation.
    Tomihata K; Suzuki M; Ikada Y
    J Biomed Mater Res; 2001; 58(5):511-8. PubMed ID: 11505425
    [TBL] [Abstract][Full Text] [Related]  

  • 9. Tensile strength of absorbable suture materials: in vitro analysis of the effects of pH and bacteria.
    Chung E; McPherson N; Grant A
    J Surg Educ; 2009; 66(4):208-11. PubMed ID: 19896625
    [TBL] [Abstract][Full Text] [Related]  

  • 10. Mechanical performance of polyglycolic acid and polyglactin 910 synthetic absorbable sutures.
    Rodeheaver GT; Thacker JG; Edlich RF
    Surg Gynecol Obstet; 1981 Dec; 153(6):835-41. PubMed ID: 6272438
    [TBL] [Abstract][Full Text] [Related]  

  • 11. Biomechanical performance of a braided absorbable suture.
    Faulkner BC; Gear AJ; Hellewell TB; Mazzarese PM; Watkins FH; Edlich RF
    J Long Term Eff Med Implants; 1996; 6(3-4):169-79. PubMed ID: 10167359
    [TBL] [Abstract][Full Text] [Related]  

  • 12. The effect of annealing treatments on the tensile properties and hydrolytic degradative properties of polyglycolic acid sutures.
    Browning A; Chu CC
    J Biomed Mater Res; 1986; 20(5):613-32. PubMed ID: 3011808
    [TBL] [Abstract][Full Text] [Related]  

  • 13. Effect of load and temperature on in vitro degradation of poly(glycolide-co-L-lactide) multifilament braids.
    Deng M; Zhou J; Chen G; Burkley D; Xu Y; Jamiolkowski D; Barbolt T
    Biomaterials; 2005 Jul; 26(20):4327-36. PubMed ID: 15683657
    [TBL] [Abstract][Full Text] [Related]  

  • 14. [In vivo studies on the tensile strength loss of absorbable synthetic threads].
    Thiede A; Lünstedt B; Sonntag HG
    Chirurg; 1980 Dec; 51(12):768-73. PubMed ID: 6258873
    [TBL] [Abstract][Full Text] [Related]  

  • 15. [Study of the hydrolytic degradation of a biodegradable copolymer].
    Sabino MA; Morales D; Ronca G; Feijoo JL
    Acta Cient Venez; 2003; 54(1):18-27. PubMed ID: 14515763
    [TBL] [Abstract][Full Text] [Related]  

  • 16. [Polydioxanon (PDS)--a new monofilar synthetic, absorbable suture material. Tensile strength studies in a controlled clinical trial on the large intestine of humans and physical parameters in in vitro tests].
    Lündstedt B; Thiede A
    Chirurg; 1983 Feb; 54(2):103-7. PubMed ID: 6406180
    [TBL] [Abstract][Full Text] [Related]  

  • 17. In vitro degradation of three-dimensional porous poly(D,L-lactide-co-glycolide) scaffolds for tissue engineering.
    Wu L; Ding J
    Biomaterials; 2004 Dec; 25(27):5821-30. PubMed ID: 15172494
    [TBL] [Abstract][Full Text] [Related]  

  • 18. A new synthetic monofilament absorbable suture made from polytrimethylene carbonate.
    Katz AR; Mukherjee DP; Kaganov AL; Gordon S
    Surg Gynecol Obstet; 1985 Sep; 161(3):213-22. PubMed ID: 3898441
    [TBL] [Abstract][Full Text] [Related]  

  • 19. Breaking strength and diameter of absorbable sutures after in vivo exposure in the rat.
    Outlaw KK; Vela AR; O'Leary JP
    Am Surg; 1998 Apr; 64(4):348-54. PubMed ID: 9544148
    [TBL] [Abstract][Full Text] [Related]  

  • 20. Biodegradation of absorbable sutures in body fluids and pH buffers.
    Freudenberg S; Rewerk S; Kaess M; Weiss C; Dorn-Beinecke A; Post S
    Eur Surg Res; 2004; 36(6):376-85. PubMed ID: 15591748
    [TBL] [Abstract][Full Text] [Related]  