  • 1. Microstructure of etched "IPS Empress" heat-pressed ceramics observed by SEM.
    Nakamoto H; Sugisawa H; Kawahara K; Takada H; Kaneko M; Nagamitsu Y; Kakehashi Y; Sato T; Igarashi T
    J Nihon Univ Sch Dent; 1996 Mar; 38(1):31-6. PubMed ID: 8648409
    [TBL] [Abstract][Full Text] [Related]  

  • 2. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics.
    Borges GA; Sophr AM; de Goes MF; Sobrinho LC; Chan DC
    J Prosthet Dent; 2003 May; 89(5):479-88. PubMed ID: 12806326
    [TBL] [Abstract][Full Text] [Related]  

  • 3. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics.
    Lin WS; Ercoli C; Feng C; Morton D
    J Prosthodont; 2012 Jul; 21(5):353-62. PubMed ID: 22462639
    [TBL] [Abstract][Full Text] [Related]  

  • 4. Effect of surface acid etching on the biaxial flexural strength of two hot-pressed glass ceramics.
    Hooshmand T; Parvizi S; Keshvad A
    J Prosthodont; 2008 Jul; 17(5):415-9. PubMed ID: 18482364
    [TBL] [Abstract][Full Text] [Related]  

  • 5. Factors affecting the shear bond strength of metal and ceramic brackets bonded to different ceramic surfaces.
    Abu Alhaija ES; Abu AlReesh IA; AlWahadni AM
    Eur J Orthod; 2010 Jun; 32(3):274-80. PubMed ID: 19903729
    [TBL] [Abstract][Full Text] [Related]  

  • 6. The transverse strength, reliability and microstructural features of four dental ceramics--Part I.
    Cattell MJ; Clarke RL; Lynch EJ
    J Dent; 1997 Sep; 25(5):399-407. PubMed ID: 9241958
    [TBL] [Abstract][Full Text] [Related]  

  • 7. Microtensile strength of composite bonded to hot-pressed ceramics.
    Della Bona A; Anusavice KJ; Shen C
    J Adhes Dent; 2000; 2(4):305-13. PubMed ID: 11317377
    [TBL] [Abstract][Full Text] [Related]  

  • 8. The biaxial flexural strength of two pressable ceramic systems.
    Cattell MJ; Knowles JC; Clarke RL; Lynch E
    J Dent; 1999 Mar; 27(3):183-96. PubMed ID: 10079624
    [TBL] [Abstract][Full Text] [Related]  

  • 9. Micromorphology of ceramic etching pattern for two CAD-CAM and one conventional feldspathic porcelain and need for post-etching cleaning.
    Onisor I; Rocca GT; Krejci I
    Int J Esthet Dent; 2014; 9(1):54-69. PubMed ID: 24757699
    [TBL] [Abstract][Full Text] [Related]  

  • 10. The influence of internal surface treatments on tensile bond strength for two ceramic systems.
    Kiyan VH; Saraceni CH; da Silveira BL; Aranha AC; Eduardo Cda P
    Oper Dent; 2007; 32(5):457-65. PubMed ID: 17910222
    [TBL] [Abstract][Full Text] [Related]  

  • 11. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic.
    Chaiyabutr Y; McGowan S; Phillips KM; Kois JC; Giordano RA
    J Prosthet Dent; 2008 Sep; 100(3):194-202. PubMed ID: 18762031
    [TBL] [Abstract][Full Text] [Related]  

  • 12. Effect of etching time and resin bond on the flexural strength of IPS e.max Press glass ceramic.
    Xiaoping L; Dongfeng R; Silikas N
    Dent Mater; 2014 Dec; 30(12):e330-6. PubMed ID: 25189110
    [TBL] [Abstract][Full Text] [Related]  

  • 13. The effect of different etching times of acidulated phosphate fluoride gel on the shear bond strength of high-leucite ceramics bonded to composite resin.
    Kukiattrakoon B; Thammasitboon K
    J Prosthet Dent; 2007 Jul; 98(1):17-23. PubMed ID: 17631170
    [TBL] [Abstract][Full Text] [Related]  

  • 14. [Effect of hydrofluoric acid etching time and resin bonding on the flexural strength of lithium disilicate glass ceramic].
    Ren DF; Luo XP
    Zhonghua Kou Qiang Yi Xue Za Zhi; 2013 Aug; 48(8):462-6. PubMed ID: 24238410
    [TBL] [Abstract][Full Text] [Related]  

  • 15. Crystallization and flexural strength optimization of fine-grained leucite glass-ceramics for dentistry.
    Chen X; Chadwick TC; Wilson RM; Hill RG; Cattell MJ
    Dent Mater; 2011 Nov; 27(11):1153-61. PubMed ID: 21930296
    [TBL] [Abstract][Full Text] [Related]  

  • 16. Effect of surface treatment on roughness and bond strength of a heat-pressed ceramic.
    Ayad MF; Fahmy NZ; Rosenstiel SF
    J Prosthet Dent; 2008 Feb; 99(2):123-30. PubMed ID: 18262013
    [TBL] [Abstract][Full Text] [Related]  

  • 17. [Microstructure and mechanical property of a new IPS-Empress 2 dental glass-ceramic].
    Luo XP; Watts DC; Wilson NH; Silsons N; Cheng YQ
    Zhonghua Kou Qiang Yi Xue Za Zhi; 2005 Mar; 40(2):147-9. PubMed ID: 15842874
    [TBL] [Abstract][Full Text] [Related]  

  • 18. Effect of post-silanization drying on the bond strength of composite to ceramic.
    Shen C; Oh WS; Williams JR
    J Prosthet Dent; 2004 May; 91(5):453-8. PubMed ID: 15153853
    [TBL] [Abstract][Full Text] [Related]  

  • 19. Influence of layer and stain firing on the fracture strength of heat-pressed ceramics.
    Uçtaşli S; Wilson HJ
    J Oral Rehabil; 1996 Mar; 23(3):170-4. PubMed ID: 8667122
    [TBL] [Abstract][Full Text] [Related]  

  • 20. Shear Bond Strength of Different CAD/CAM Ceramics: Acid vs Er:YAG Laser Etching.
    Hou Y; Shen R; Chen L; Chen Y; Jiang Y; Li J; Gao J
    Photomed Laser Surg; 2018 Nov; 36(11):614-620. PubMed ID: 30227090
    [TBL] [Abstract][Full Text] [Related]  