  • Title: Clinical comparison between a resin-reinforced self-cured glass ionomer cement and a composite resin for direct bonding of orthodontic brackets. Part 2: Bonding on dry enamel and on enamel soaked with saliva.
    Author: Cacciafesta V, Bosch C, Melsen B.
    Journal: Clin Orthod Res; 1999 Nov; 2(4):186-93. PubMed ID: 10806942.
    Abstract:
    The purposes of this investigation were to compare the clinical performance of a resin-reinforced self-cured glass ionomer cement to a standard composite resin in the direct bonding of orthodontic brackets when bonded onto: a) dry teeth and b) teeth soaked with saliva. The two bonding agents were compared using a split-mouth design. In that, both systems were used for direct bonding of stainless steel brackets in every patient. Thirty-eight consecutive patients with fixed appliances were followed for a period of 12 months. The patients were randomly divided into two groups: group A (11 patients) and group B (27 patients). In group A, the performance of 220 stainless steel brackets was evaluated: 110 brackets were bonded with GC Fuji Ortho glass ionomer cement (GC Industrial Co., Tokyo, Japan) onto dry teeth, and 110 bonded with System 1+ composite resin (Ormco Corp., Glendora, CA). In group B, the performance of 540 stainless steel brackets was evaluated: 270 brackets were bonded with GC Fuji Ortho onto teeth soaked with saliva, and 270 bonded with System 1+. In group A, GC Fuji Ortho recorded an overall failure rate (34.5%) significantly higher (p < 0.05) than System 1+ (9%) when applied onto completely dry teeth. Conversely, in group B, no statistically significant differences (p > 0.05) between the failure rates of the two bonding agents were found when GC Fuji Ortho was used on teeth soaked with saliva. It was concluded, therefore, that GC Fuji Ortho shows clinically acceptable bond strengths when bonded onto moist teeth, but not when used on dry enamel. Both bonding agents failed mostly at the enamel/adhesive interface, without causing any enamel damage.
    [Abstract] [Full Text] [Related] [New Search]