These tools will no longer be maintained as of December 31, 2024. Archived website can be found here. PubMed4Hh GitHub repository can be found here. Contact NLM Customer Service if you have questions.


PUBMED FOR HANDHELDS

Search MEDLINE/PubMed


  • Title: Dentin bond strengths as a function of solvent and glutaraldehyde content.
    Author: Ritter AV, Bertoli C, Swift EJ.
    Journal: Am J Dent; 2001 Aug; 14(4):221-6. PubMed ID: 11699741.
    Abstract:
    PURPOSE: To evaluate the effect of the inclusion of glutaraldehyde on the shear bond strength of new ethanol-based adhesives (Gluma Comfort Bond & Desensitizer, GCBD and Gluma Comfort Bond, GCB) versus acetone-based Gluma One Bond (GOB) and a conventional three-step adhesive as a control. MATERIALS AND METHODS: Forty bovine incisors were mounted in acrylic, polished to 600-grit, and randomly assigned to four groups (n=10). Dentin was etched for 15 s using 35% phosphoric acid, rinsed, and lightly dried. After adhesive application and curing, Charisma composite was applied in a #5 gelatin capsule and light-cured. Specimens were loaded in shear using an Instron at 5 mm/min. Shear bond strengths were calculated by dividing failure load by bonded surface area. ANOVA showed a significant difference in means at P< 0.01, so Tukey's test was used for pairwise comparisons. RESULTS: Mean SBS (+/- SD, MPa) were: GOB: 8 (4.4)ab; GCB: 10 (4.4)ab; GCBD: 14 (6)bc; SBMP: 17.7 (6.4)c. Superscript letters indicate Tukey's homogeneous subsets (P< 0.05).
    [Abstract] [Full Text] [Related] [New Search]