  • Title: Bond strength to primed Ti-6Al-7Nb alloy of two acrylic resin adhesives.
    Author: Koizumi H, Furuchi M, Tanoue N, Yanagida H, Yoneyama T, Matsumura H.
    Journal: Dent Mater J; 2006 Jun; 25(2):286-90. PubMed ID: 16916231.
    Abstract:
    This study aimed to evaluate the bonding behavior of two acrylic resin adhesives joined to titanium-aluminum-niobium (Ti-6Al-7Nb) alloy primed with two metal conditioners. Cast Ti-6Al-7Nb alloy disks were air-abraded with alumina and bonded with six combinations of two resin adhesives (Super-Bond C&B and Multi Bond) and three surface conditions (Alloy Primer, M.L. Primer, and unprimed control). Shear bond strengths were determined both before and after 20,000 thermal cycles. The tri-n-butylborane initiated Super-Bond C and B resin exhibited greater bond strength than the BPO-amine initiated Multi-Bond resin. Both the Alloy Primer with a hydrophobic phosphate and the M.L. Primer with a phosphonoacetate effectively improved the 24-hour bond strength of Multi-Bond resin as well as the post-thermocycling bond strength of Super-Bond C and B resin.
    [Abstract] [Full Text] [Related] [New Search]