  • Title: Effect of bleaching on microhardness of esthetic restorative materials.
    Author: Malkondu Ö, Yurdagüven H, Say EC, Kazazoğlu E, Soyman M.
    Journal: Oper Dent; 2011; 36(2):177-86. PubMed ID: 21702674.
    Abstract:
    This study evaluated the effect of a high-concentration carbamide peroxide–containing home bleaching system (Opalescence PF) and a hydrogen peroxide–containing over-the-counter bleaching system (Treswhite Supreme) on the microhardness of two nanocomposites (Filtek Supreme XT and Premise) and leucite-reinforced glass ceramic (Empress Esthetic), glass ceramic (Empress 2 layering), and feldspathic porcelain (Matchmaker MC). A total of 100 specimens, 20 of each kind of the restorative materials, 2 mm in thickness and 10 mm in diameter, were fabricated. Then the specimens were polished with SiC paper and 1 μm alumina polishing paste. After polishing, porcelain specimens were glazed in accordance with the manufacturer's instructions. Each type of restorative material was then randomly divided into two groups (n=10), and the specimens were treated with either Opalescence PF or Treswhite Supreme. The microhardness of the specimens before bleaching (baseline) and after bleaching was determined using a digital microhardness tester. Data were analyzed using the Mann-Whitney U-test and the Wilcoxon test. Opalescence PF significantly influenced the hardness of all the restorative materials. Statistically significant decreases with respect to before bleaching were found for Premise (p=0.005), Empress Esthetic (p=0.003), Empress 2 layering (p=0.005), and Matchmaker-MC (p=0.003), whereas a statistically significant increase was observed in Filtek Supreme XT (p=0.028). The difference in the microhardness values between before and after bleaching using Treswhite Supreme was statistically significant only for Premise (p=0.022). High-concentration carbamide peroxide–containing home bleaching may affect the microhardness of restorative materials.
    [Abstract] [Full Text] [Related] [New Search]