These tools will no longer be maintained as of December 31, 2024. Archived website can be found here. PubMed4Hh GitHub repository can be found here. Contact NLM Customer Service if you have questions.


PUBMED FOR HANDHELDS

Search MEDLINE/PubMed


  • Title: The Surface Roughness of Contemporary Indirect CAD/CAM Restorative Materials That Are Glazed and Chair-Side-Finished/Polished.
    Author: Albani R, Habib SR, AlQahtani A, AlHelal AA, Alrabiah M, Anwar S.
    Journal: Materials (Basel); 2024 Feb 21; 17(5):. PubMed ID: 38473470.
    Abstract:
    The surface roughness (Ra) of indirect computer-aided design/computer-aided manufacturing (CAD/CAM)-fabricated dental restorations is crucial for their long-term durability. This study intended to evaluate the Ra of five different types of contemporary indirect CAD/CAM restorative materials with varying compositions that were glazed and finished/polished. A total of 75 specimens, disc-shaped (10 mm × 2 mm), were obtained from five materials (n = 15) (Tetric CAD, IPS e.max CAD, IPS e.max ZirCAD, CELTRA Duo, and Vita Enamic) and fabricated by CAD/CAM. One of the two surfaces for each specimen was subjected to glazing, while the other surface was subjected to finishing/polishing. The Ra of the two surfaces in micrometers (μm) was evaluated using a Profilometer, while the surface topography was examined using a scanning electron microscope. Using SPSS, the Kruskal-Wallis, post hoc Conover, and Mann-Whitney tests were used to statistically evaluate the data. A comparison of the Ra for the finished/polished surfaces of the five test materials showed significant differences (p < 0.0001). Among the finished/polished surfaces, the mean rank values of Vita Enamic were significantly higher than the other four test materials (p < 0.0001). A comparison of the Ra of glazed surfaces among the five study materials revealed significant differences (p < 0.0001). The Ra for the IPS e.max ZirCAD material was significantly higher than the rest of the four materials (p < 0.001). A comparison of the Ra for two types of surface conditioning within each of the five test materials showed a significant difference (p < 0.05). Only for IPS e.max ZirCAD was the Ra of the glazed surface significantly higher than the finished/polished surface (p < 0.0001). Significant variations in the surface roughness (Ra) were exhibited between the finished/polished and glazed surfaces of the five test materials. Hybrid ceramics showed the highest Ra values for the finished/polished surfaces, and zirconia exhibited the highest Ra values among the glazed surfaces among the tested materials. The Ra values of either finished/polished or glazed surfaces of the test materials were within the clinically acceptable range (0.2-0.5 μm), except for the glazed surface of the zirconia ceramics (0.84 μm).
    [Abstract] [Full Text] [Related] [New Search]