1. Impact of high-speed sintering, layer thickness and artificial aging on the fracture load and two-body wear of zirconia crowns. Wiedenmann F, Pfefferle R, Reichert A, Jerman E, Stawarczyk B. Dent Mater; 2020 Jul; 36(7):846-853. PubMed ID: 32414506 [Abstract] [Full Text] [Related]
2. Impact of the material and sintering protocol, layer thickness, and thermomechanical aging on the two-body wear and fracture load of 4Y-TZP crowns. Mayinger F, Buser R, Laier M, Schönhoff LM, Kelch M, Hampe R, Stawarczyk B. Clin Oral Investig; 2022 Nov; 26(11):6617-6628. PubMed ID: 35840737 [Abstract] [Full Text] [Related]
3. Impact of High-Speed Sintering of Three-Unit 3Y-TZP and 4Y-TZP Fixed Dental Prostheses on Fracture Load With and Without Artificial Aging. Mayinger F, Pfefferle R, Reichert A, Stawarczyk B. Int J Prosthodont; 2021 Nov; 34(1):47-53. PubMed ID: 33570519 [Abstract] [Full Text] [Related]
7. Mechanical performance of cement- and screw-retained all-ceramic single crowns on dental implants. Obermeier M, Ristow O, Erdelt K, Beuer F. Clin Oral Investig; 2018 Mar; 22(2):981-991. PubMed ID: 28710653 [Abstract] [Full Text] [Related]
8. Impact of high-speed sintering on translucency, phase content, grain sizes, and flexural strength of 3Y-TZP and 4Y-TZP zirconia materials. Jansen JU, Lümkemann N, Letz I, Pfefferle R, Sener B, Stawarczyk B. J Prosthet Dent; 2019 Oct; 122(4):396-403. PubMed ID: 30982619 [Abstract] [Full Text] [Related]
9. In vitro investigation of fracture load and aging resistance of high-speed sintered monolithic tooth-borne zirconia crowns. Nakamura T, Nakano Y, Usami H, Okamura S, Wakabayashi K, Yatani H. J Prosthodont Res; 2020 Apr; 64(2):182-187. PubMed ID: 31699614 [Abstract] [Full Text] [Related]
10. Influence of CAD/CAM Fabrication and Sintering Procedures on the Fracture Load of Full-Contour Monolithic Zirconia Crowns as a Function of Material Thickness. Zimmermann M, Ender A, Mehl A. Oper Dent; 2020 Apr; 45(2):219-226. PubMed ID: 31738694 [Abstract] [Full Text] [Related]
11. Impact of high-speed sintering on accuracy and fit of 4 mol% yttria-stabilized tetragonal zirconia polycrystals (4Y-TZPs). Antón X, Stawarczyk B, Reymus M, Joda T, Liebermann A. Int J Prosthodont; 2021 Apr; 34(6):775–783. PubMed ID: 33616554 [Abstract] [Full Text] [Related]
12. Influence of different surface treatments on two-body wear and fracture load of monolithic CAD/CAM ceramics. Wiedenmann F, Böhm D, Eichberger M, Edelhoff D, Stawarczyk B. Clin Oral Investig; 2020 Sep; 24(9):3049-3060. PubMed ID: 31836916 [Abstract] [Full Text] [Related]
13. In vitro performance of full-contour zirconia single crowns. Beuer F, Stimmelmayr M, Gueth JF, Edelhoff D, Naumann M. Dent Mater; 2012 Apr; 28(4):449-56. PubMed ID: 22196898 [Abstract] [Full Text] [Related]
14. Evaluation of wear behavior of dental restorative materials against zirconia in vitro. Maier E, Grottschreiber C, Knepper I, Opdam N, Petschelt A, Loomans B, Lohbauer U. Dent Mater; 2022 May; 38(5):778-788. PubMed ID: 35459553 [Abstract] [Full Text] [Related]
15. Fatigue and wear behaviour of zirconia materials. Rosentritt M, Preis V, Behr M, Strasser T. J Mech Behav Biomed Mater; 2020 Oct; 110():103970. PubMed ID: 32957257 [Abstract] [Full Text] [Related]
16. Influence of different surface finishing procedures of strength-gradient multilayered zirconia crowns on two-body wear and fracture load: Lithium silicate or leucite glazing versus polishing? Hoffmann M, Mayinger F, Stawarczyk B. J Mech Behav Biomed Mater; 2024 Feb; 150():106307. PubMed ID: 38071838 [Abstract] [Full Text] [Related]
17. Impact of the sintering parameters on the grain size, crystal phases, translucency, biaxial flexural strength, and fracture load of zirconia materials. Mayinger F, Ender A, Strickstrock M, Elsayed A, Nassary Zadeh P, Zimmermann M, Stawarczyk B. J Mech Behav Biomed Mater; 2024 Jul; 155():106580. PubMed ID: 38759588 [Abstract] [Full Text] [Related]
18. Load-bearing capacity of CAD/CAM 3D-printed zirconia, CAD/CAM milled zirconia, and heat-pressed lithium disilicate ultra-thin occlusal veneers on molars. Ioannidis A, Bomze D, Hämmerle CHF, Hüsler J, Birrer O, Mühlemann S. Dent Mater; 2020 Apr; 36(4):e109-e116. PubMed ID: 31992483 [Abstract] [Full Text] [Related]
19. Influence of speed sintering on the fit and fracture strength of 3-unit monolithic zirconia fixed partial dentures. Elisa Kauling A, Güth JF, Erdelt K, Edelhoff D, Keul C. J Prosthet Dent; 2020 Sep; 124(3):380-386. PubMed ID: 31780110 [Abstract] [Full Text] [Related]